Tang Lian Chemistry

Performance parameters of glass lined disc condenser

The performance parameters of glass lined disc condenser vary depending on the model and specifications, but usually include the following aspects

Design pressure and temperature: The design pressure inside the device is generally -0.1MPa to 0.25MPa, and the design pressure of the interlayer is 0.25MPa to 0.35MPa; The design temperature range is usually from -20 ℃ to 200 ℃.

Heat transfer coefficient: The heat transfer coefficient is relatively high, generally reaching 485Kcal/hm ² C, which helps to improve condensation efficiency.

Ceramic layer thickness and voltage resistance: The ceramic layer thickness is usually between 0.8mm and 2.0mm, and the voltage resistance can reach 20KV, ensuring the safety and durability of the equipment.

Condensation area and model: The condensation area varies depending on the model, such as 0.5 square meters per piece for P0.5 type and 1 square meter per piece for P1 type. It can be flexibly selected according to production needs.

glass lined disc condenser

These performance parameters collectively determine the condensation efficiency and service life of the glass lined disc condenser.

Glass lined disc condenser is a commonly used condensing equipment in the chemical and pharmaceutical industries, with the following characteristics:

  1. Efficient heat transfer: Heat exchange occurs through the reverse flow of hot air and cooling water, resulting in high heat transfer efficiency.
  2. Not easy to scale: The design is reasonable, not easy to scale, and the heat exchange efficiency is greatly improved.
  3. Strong adaptability: able to handle various chemical media, such as hydrofluoric acid, phosgene, concentrated phosphoric acid, etc.
  4. Compact structure: small size, light weight, compact structure, easy to install and maintain.

In addition, the glass lined disc condenser also has strong compressive strength and other performance characteristics, which can be used in higher vacuum distillation devices to improve problems such as pressure drop and leakage.

When using, attention should be paid to assembling according to the drawings and relevant requirements.

Sharp or hard substances are strictly prohibited from colliding or rubbing against the enamel surface to prevent damage to the equipment.

For condensers with slight leakage, welding technology can be used for repair. If the damage is severe, the entire condenser component needs to be replaced.