Enamel equipment these materials can not be used

Enameled equipment, with excellent corrosion resistance, but the following appear several kinds of materials when the corrosion resistance of enameled equipment is not so useful.

The first case, any concentration and temperature of hydrofluoric acid and contain fluoride ion media or materials.

The second case, the concentration is greater than 30%, the temperature is higher than 180 ℃ phosphoric acid medium or material.

The third case, PH value greater than 12 and temperature higher than 80 ℃ alkaline media or materials.

The fourth case, acid and alkaline materials alternating reaction process.

In which the first case of any concentration and temperature of hydrofluoric acid and contain fluoride ions of the medium or material is the enamel equipment is the most intolerant and most afraid of the use of such materials, if the use of such materials, a few days time will make the enamel on the surface of the enamel layer erosion of light, that is, the loss of due luster, but also greatly reduces the enamel surface of the corrosion resistance of the use of its time is greatly reduced, the whole enamel glass layer will corrode off and thus very quickly to the carbon steel body corrosion off. Body corrosion. The whole enamel equipment scrapped.

Therefore, remember not to add such materials in the enamel equipment.